05/Screening
Release time: 2019-11-05 16:24:00.000
source:
The traditional screening method for foundry sand is called three-screening method, which means that the concentration of three consecutive sieves is more than 75%. But this could not satisfy the need of the ceramic Sand, which is concentration of single sieve is more than 85%, and residual of two consecutive sieves is less than 15%. Because of the negative effect from the aluminum carbonate fiber and iron, the result of the screening is as follows:
14Mesh: 0.141mm 70Mesh: 0.212mm
20Mesh: 0.85mm 100Mesh: 0.153mm
30Mesh: 0.6mm 140Mesh: 0.105mm
36Mesh: 0.425mm 200Mesh: 0.073mm
50Mesh: 0.3mm Over 200Mesh
More News
Problems in Casting Process of Lost Foam Casting
Lost foam casting (LFC) process has been developed rapidly in recent years because of its low investment and low cost.The gating system plays a very important role in the lost foam casting process, an
The V process casting originated in Japan. It uses plastic film to vacuum to make dry sand molding, that is, physical modeling.Because it does not use binder, shakeout is simple and convenient, the co
It has become a trend for foundry industry to move from tradition to intelligence
It has become a trend for foundry industry to move from tradition to intelligence.The typical application mode of intelligent casting is digital foundry, which uses information technology to manage al
多行文本内容元素
富文本内容绑定数据后可解析HTML语言内容
LUOYANG RUIYU CERAMIC SAND CO., LTD.
Tel:+86 379 65110927
Fax:+86 379 65110921
Email:lyry@lyruiyu.cn
Website:www.lyruiyu.cn www.foundry-sand.cn
Address: Gaolong Town, Yanshi county, Luoyang, Henan, China

Mobile site

WeChat public account